$ÐLùî#Studyonelectrochemicalpolishingof316LstainlesssteelstentJI Shi-wei, H UAN G Nan* , WAN Guo-j iang, WAN G Kai( Key Laboratory of Advanced Technology of Materials, Ministry Education,Southwest Jiaotong University, Chengdu 610031, China)ABSTRACT This research focuses on DC-electrochemical polishing of 316L stainless steel stent materials. Functions ofthe components in electrochemical polishing solutions were studied. T he effect of operating conditions on polishing qualitywas investigated. High smooth surface can be obtained quickly.KEYWORDS 316L stainless steel; Stent; Electrochemical polishing316LÑÓ5¦OÈÄÐ;ý\ùî季士委,黄 楠* ,万国江,王 凯(2YvÐ5É/â×ÄLi,¹+îû 610031)[K 1] ¨°@ÈÄÐ;/,ùî316LÑÓ5¦OÈÄÐ;AÏòîs¥T¨# THq;É¥Y bYVªÄ,¨L¤¥ý\? y¤;Ü¥;Vë b[1oM] 316LÑ;¦O;ÈÄÐ;[Ïms Ë|] TH142 [ÓDSM] A [ÓcI|] 1672-8475(2006)03-0217-04[Á["]SE1 SÐÁÏ-ÖT["( 30318006) ;¹+8S=T["( 05HH0023) b[Teº]1V¾( 1982- ) ,3,~?û¦,«V bE- mail: Zdjsw @163. com[YßT]Û,2YvÐ5É/â×ÄLi,610031 bE-mail: nhuang@ 263. net[là°ù] 2005-12-15 [©í°ù] 2006-02-270 ý-,3îhMXÜ^¯}¦ Ë3¥ô'¥ðyB[ 1] bÛ"ºÆÍ/¥?Z,Ó5=Á¦O¥ùÅEs¦ô" bÏ316LÑT¹Ó5¦O¥¨Xܵ É åN bÁ¦O¥ÁÓX$£L^¦O±ÆªYh¦ B¯¥×1yÍ bùîsVü,Y¦OÐÓAM¸¥yÍ,ö1y͹VëY¡ bVëY¡ v,]ÓAÏ¥ë v,`Ó¥ V? v[ 2] b®¿Ó5¦O²¯ ajl,¨;Mé©ZTîYFýª,VëÚ¨¦ý;X V?[ 3] bÈÄÐ;[1&ªÄ$ª5 In¨¿¦O¥VëÚ[ 4] b'Ó¨°@ÈÄÐ;¥ZE,316LÑÓ5¦OÉVëÚý\ùî bìBÕ¨¿D¨Ñ±Æ¥L¨ aÚr¥VëÚý\,^íÂ316LŦýÓ5¦O¥VëÈÄÐ; bm1 LÂUim1 LZE1. 1L Âm1îU,¾L®ȳ¢ aF£Â aÑ9 a|(Ñ) aó a°@È÷#ÏÄLFî bÈ÷¥¤$;k"() bó)¿Aëð/Z bȳARþ,?#217#ÏSºÆ^ÐÍÐ2006M»3 »3ù Chin J Interv Imaging Ther, 2006, Vol 3, No 3öÀ"Ö' V,"µù¿¥¨ æd bW [3~ 5 cm¹D b1. 2ý\@ñ ÈÑÄÐ"² ¹b! ¹Äà ¹b! ¹ÈÄÐ; ¹b! ¹Ï ¹b! ¹Ä ¹b! ¹Ä2i b1. 2. 1k"Å! ¨È½LMéE|316LÑÅî°å¹12 mm¥Ë,100#Yé¼uª,GQ280# a400# a600# a800#¥£é¼Y¡Ra 0. 16~ 0. 08 Lm b¨; YK316LÑõ5,ªÖÏ,Ñ2ob!,ÜM",'¤L¨Ó5¦O b1. 2. 2ÄÐ"²¥ZÖ) 20 g/ L_Ä) 15 g/ LÖ) 20 g/ LÄÄ4(OP-10) 10 ml/LÑ ÈÑHW 10 min1. 2. 3ÄÃ10%;Ö 10 min1. 2. 4ÏA5%Ö_)·A 2~ 3 min1. 2. 5ÄA×ðÖK 18 g/ L_Ä) 3 g/LpH´ 6. 5~ 7. 5HW 5~ 10 min1. 3_ZE1. 3. 1A±ä4³ ;ªA±ä/4³,Vüíà aíM aíZ_,Ü; b1. 3. 20ªK £SZahner³IM6ÈÄÐýT_É,¨îÈÊE©ÈÄÐ;ª¥Vë(E)Hanks·AÏ¥ÄwL,]H©;Ñ(M)¥ÄwLÉ1 b1. 4;A¥Z a THq#ÿiY[1. 4. 1;A¥Z# THqÖ(85%) 650 ml/L;Ö(98%) 250 ml/LØÄð 80 g/ L@F4 10 g/ LÑ 70~ 80eÈâ 18 VHW 2 min|ë 4B1| Ñ1. 4. 2ÿiY[ æ¥Â;AVñÏÿiòîs¥Fƨ½,¥î·A¥ØÄð5FÆÖÏ,ó (ªF;Ö, ϪF@F4 b çSBç¥Lª,;Aö>r,s÷÷Ð b2 ²TÐ)2. 1ÈÄÐ;AÏòîs¥T¨#Y2. 1. 1Ö Ö^;A¥ö1îs,;VñÏ,;?·³T¨,»?ÑVëîÖ÷¹,E¸ÑVë?3VªK[ 5] bÖcÊ®,;A1×l,*l, Ö0 ÛÎF y,Á·³F y, æ¿rÜ;rT;ÖcVÚ,5î'VÚ,O;¤ bL²TVü,Öc650 ml/ LH,;rTrKz b²TnV1 bV1 Öc;É¥YÖ( ml/ L);Vë 560k"Vëܵ,;µ590k"VëÜBî,;µ620k"VëÜ,;Bî650k"VëÜ,;680k"VëÜ,;2. 1. 2;Ö ;Ö^;AFî¥Bs b;ý\ÏÀµÿP¨;Ö¥f ,ðy^ÿ¨;ÖH,¥·³v¥;Ö÷Ö8|E¸;ÉB¥É[ 5] b;Öµù¿4Ú;A¥Èq,4ÚsÛ? ïÈ@rq bFÆa¥;Öµù¿ÅÖVëÜ,4ÚVë;,;ÖcV®,ÅÖ4[Ü;;ÖcVÚ,ö®Vë;±,êÈ;A¥P¨p bL²TVü,;Öc¹250 ml/ LH,8rTKD b²TnV2 bV2 ;Öc;É¥Y;Ö( ml/ L);Vë 190k"Vëܵ,;µ210k"VëÜBî,; µ230k"VëÜ,;Bî250k"Ü,;270k"Ü,;2. 1. 3ØÄð CrO3^ÿ¨ Sȳ;#218#ÏSºÆ^ÐÍÐ2006M»3 »3ù Chin J Interv Imaging T her, 2006, Vol 3, No 34¥,ÈÈ^FðîsÏP¨,Â;Ö aÖÏFBtCrO3¥î;·A bȳAÏFÆCrO3[ª V[¤z¥;rT bÄÕcCrO3¥È³A,1¤z¥;²T,ûA¶»ûBç¥Cr2 O7 2+。